GRTRANSFER25

Easy transfer monolayer Graphene

L × W 1 in. × 1 in., avg. no. of layers, 1

Manufacturer: Sigma Aldrich

Select a Size

Pack Size SKU Availability Price
1 EACH GRTRANSFER25-1-EACH In Stock ₹ 20,091.20

GRTRANSFER25 - 1 EACH

₹ 20,091.20

In Stock

Quantity

1

Base Price: ₹ 20,091.20

GST (18%): ₹ 3,616.416

Total Price: ₹ 23,707.616

feature

avg. no. of layers 1

growth mode

CVD

sheet resistance

450 +/- 40 Ω/sq, on SiO2/Si (1cm x 1cm)

L × W

1 in. × 1 in.

surface coverage

>98%

color

transparent>97%

grain size

≤20 μm

Related Products

Img

Sigma Aldrich

GRTRANSFER10

L × W 1 cm × 1 cm, avg. no. of laye...

Img

Sigma Aldrich

773700

1 cm x 1 cm on SiO2/Si substrate, a...

Img

Sigma Aldrich

773719

1 cm x 1 cm on quartz, avg. no. of ...

Img

Sigma Aldrich

920118

4 in diameter, avg. no. of layers, ...

Img

Sigma Aldrich

900442

dispersion in DMF, avg. no. of laye...

Img

Sigma Aldrich

652482

80-90% carbon basis, D × L 2-10 nm ...

Img

Sigma Aldrich

920126

4 in diameter, avg. no. of layers, ...

Img

Sigma Aldrich

920134

6 in diameter, avg. no. of layers, ...

Description

  • General description: A 1 in x 1 in CVD grown monolayer CVD graphene (verified by Raman 2D/G ratio) is sandwiched between a scarificial layer and a water-releasable polymer support film.Structure of the easy-transfer graphene:Top sacrificial layer (square shaped), CVD monolayer graphene in the middle, and bottom water-releasable polymer support layer (round shaped)
  • Application: A clean way to trasfer monolayer graphene is highly desired for the utilization of its exceptional properties. This product employs a specially designed mechanism for easy and clean transfer of high quality monolayer CVD grown graphene to build state-of-art electronic devices such as:Graphene based state-of-art FETGraphene based sensorsHeterostructure based micro/nano electronicsClean tranfer can be done following below 3 easy steps: Release Put the sample on deionized(DI) water slowly, round side (polymer layer) facing down, the square-shaped sacrificial layer+graphene will gradually detach from the rorund polymer film. Once the sacrificial layer/graphene is floating remove the round polymer film.TransferBring the desired substrate into the same DI water container while the sacrificial layer/graphene is floating. Tilt the substrate 45º and bring it into contact with the sacrificial layer/graphene from below. Take the sacrificial layer/graphene/substrate out and let it dry for 30 minutes in air. Then anneal the samples on a hot plate at 150 Celsius for 1h. Finally, before removing the sacrificial layer, store it under vacuum for at least 24h to avoid detachment of the graphene from your substrate.Sacrificial layer RemovalTo remove the sacrificial layer two methods can be used:Solvents: Dip the sacrificial layer/graphene/substrate in acetone for 1h, then into isopropyl alcohol for another 1h and blow the sample with N2 to dry it.Thermal treatment: Put the sacrificial layer/graphene/substrate into an oven and heat the sample at 450 C ininert atmosphere for 2h.

SAFETY INFORMATION

WGK

WGK 1

Flash Point(F)

Not applicable

Flash Point(C)

Not applicable

Compare Similar Items

Show Difference

Img

Sigma Aldrich

GRTRANSFER25

L × W 1 in. × 1 in., avg. no. of la...


feature:
avg. no. of layers 1

growth mode:
CVD

sheet resistance:
450 +/- 40 Ω/sq, on SiO2/Si (1cm x 1cm)

L × W:
1 in. × 1 in.

surface coverage:
>98%

color:
transparent>97%

grain size:
≤20 μm

Img

Sigma Aldrich

GSS-1015

The GS System (offered by & a regis...


feature:
__

growth mode:
__

sheet resistance:
__

L × W:
__

surface coverage:
__

color:
__

grain size:
__

Img

Sigma Aldrich

GSS-1016

The GS System (offered by & a regis...


feature:
__

growth mode:
__

sheet resistance:
__

L × W:
__

surface coverage:
__

color:
__

grain size:
__

Img

Millipore

GSTF01300

MF-Millipore™, filter diam. 13 mm, ...


feature:
hydrophilic

growth mode:
__

sheet resistance:
__

L × W:
__

surface coverage:
__

color:
white

grain size:
__